ℹ️
🇬🇧
Search
Search for people relevant for "mikrostruktura"
mikrostruktura
Person
Class
Person
Publication
Programmes
Export current view
doc. RNDr. Martin Vlach Ph.D.
Academic staff at Faculty of Mathematics and Physics
7 classes
122 publications
Classes
class
Introduction to Measurement in Physics
+1
NFUF102 |
Faculty of Mathematics and Physics
class
Physics in Experiments I
NOFY067 |
Faculty of Mathematics and Physics
class
Physics in Experiments II
NOFY068 |
Faculty of Mathematics and Physics
class
Selected Topics on Physics II
NUFY037 |
Faculty of Mathematics and Physics
class
Selected parts of solid state physics I
NUFY128 |
Faculty of Mathematics and Physics
class
Selected parts of solid state physics II
NUFY129 |
Faculty of Mathematics and Physics
Publications
publication
Characterization of phase development in non-isothermally annealed mould-cast and heat-treated Al-Mn-Sc-Zr alloys
2010 |
Faculty of Mathematics and Physics
publication
Influence of Mn on mechanical properties and microstructure of mould-cast Al-Sc-Zr-based alloy
2010 |
Faculty of Mathematics and Physics
publication
Response of mould-cast and cold-rolled ternary Al-Sc-Zr alloy to isochronal annealing
2009 |
Faculty of Mathematics and Physics
publication
Defect studies of hydrogen loaded Nb: bulk metals and thin films
+1
2007 |
Faculty of Mathematics and Physics
publication
Effect of heat treatment on microstructure and properties of cast and deformed Al alloys with addition of Yb, Er and Zr
2023 |
Faculty of Mathematics and Physics
publication
Effect of deformation on evolution of Al-3(Er,Zr) precipitates in Al-Er-Zr-based alloy
2022 |
Faculty of Mathematics and Physics
publication
On the Sc-rich core of Al-3(Sc,Er,Zr) precipitates
2022 |
Faculty of Mathematics and Physics
publication
Electrical Resistivity of Binary Mg Alloys
2022 |
Faculty of Mathematics and Physics
publication
Phase transformations in commercial cold-rolled Al-Zn-Mg-Cu alloys with Sc and Zr addition
2021 |
Faculty of Mathematics and Physics
publication
Heat Treatment of Cast and Cold Rolled Al-Yb and Al-Mn-Yb-Zr Alloys