Addition of metal chlorides to a HOCl conditioner can enhance bond strength to smear layer deproteinized dentin

Publikace na 1. lékařská fakulta |
2022

Tento text není v aktuálním jazyce dostupný. Zobrazuje se verze "en".Abstrakt

Objectives: To evaluate the effect of smear layer deproteinization using hypochlorous acid (HOCl) with/without metal chlorides (SrCl2 and ZnCl2) on the microtensile bond strength (µTBS) of two simplified adhesives to dentin. Methods: Human dentin surfaces with a standardized smear layer were pretreated using a 105 ppm HOCl solution with/without SrCl2 (0.05 M, 0.1 M, 0.2 M, 0.4 M) or ZnCl2 (0.05 M, 0.1 M, 0.2 M) for 5 s, 15 s, or 30 s.

After the deproteinizing solution was washed out with water for 5 s, 15 s, or 30 s, pretreated surfaces were bonded with one-step self-etch adhesive Bond Force II or universal adhesive Clearfil Universal Bond Quick, and µTBS was measured after 24 h. Additionally, the deproteinizing effects of HOCl solutions with/without the metal chlorides were compared by measuring changes in the amide:phosphate ratio using attenuated total reflection Fourier transform infrared spectroscopy.

Statistical analysis was performed using multifactor ANOVA, Tukey's post hoc tests and t-tests (p 0.05). Significance: The effectiveness of smear layer deproteinization using HOCl can be improved by the addition of metal chlorides, as their increasing concentration allowed to shorten the wash-out time from 30 s down to 5 s.